Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flame Spread | 24 mm/min @Thickness 1.00 mm |
0.94 in/min @Thickness 0.0394 in |
ISO 3795 (FMVSS 302) |
DuPont Performance Polymers Crastin® S600F20 BK851 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l Unreinforced Medium Viscosity Polybutylene Terephthalate Crastin S600F20 BK851 is an unreinforced lubricated medium viscosity black polybutylene terephthalate resin for injection molding.Information.. |
|||
Flame Spread | 24 mm/min @Thickness 1.00 mm |
0.94 in/min @Thickness 0.0394 in |
ISO 3795 (FMVSS 302) |
DuPont Performance Polymers Hytrel® DYM250S BK472 TPC-ET+PBT
(Unverified Data**) Medium Modulus Polyester Elastomer with Excellent Impact Resistance Developed for Air Bag Door ApplicationsHytrel DYM250S BK472 is a medium modulus resin suited for injection molding of Air Bag Depl.. |
|||
Flame Spread | 24 mm/min @Thickness 1.00 mm |
0.94 in/min @Thickness 0.0394 in |
SE/B24; ISO 3795 (FMVSS 302) |
DuPont Performance Polymers Zytel® 70G30HSLR BK099 Nylon 66
(Unverified Data**) 30% Glass Reinforced Heat Stabilized Hydrolysis Resistant Polyamide 66 Zytel 70G30HSLR BK099 is a 30% glass fiber reinforced heat stabilized hydrolysis resistant polyamide 66 resin for injection mol.. |
|||
Flame Spread | 24 mm/min @Thickness 1.00 mm |
0.94 in/min @Thickness 0.0394 in |
ISO 3795 (FMVSS 302) |
DuPont Performance Polymers Zytel® FE270050 BK099 Nylon 66
(Unverified Data**) 30% Glass/Mineral Reinforced Polyamide 66Information provided by DuPont Performance Polymers |
|||
Flame Spread | 24 mm/min @Thickness 1.00 mm |
0.94 in/min @Thickness 0.0394 in |
SE/B; ISO 3795 (FMVSS 302) |
DuPont Performance Polymers Crastin® SO653 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) 20% Glass Bead Filled Polybutylene Terephthalate with Low Warpage CharacteristicsCrastin SO653 NC010 is a 20% glass bead filled polybutylene terephthalate resin for injection molding. It has isotrop.. |
|||
Flame Spread | 24 mm/min @Thickness 1.00 mm |
0.94 in/min @Thickness 0.0394 in |
ISO 3795 (FMVSS 302) |
DuPont Performance Polymers Zytel® 79G13HSL BK039 Nylon 66
(Unverified Data**) 13% Glass Reinforced Toughened Heat Stabilized Polyamide 66 Zytel 79G13HSL BK039 is a 13 % glass reinforced heat stabilized lubricated slightly toughened black polyamide 66 for injection molding. It.. |