Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flame Spread | 22.0 - 22.1 mm/min | 0.866 - 0.870 in/min | Average value: 22.1 mm/min Grade Count:4 |
Overview of materials for Polypropylene, Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Mineral Reinforced". Each property range of values reported is minimum and maximum values.. |