Polymer Property : Flame Spread = 2.5 in/min Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Flame Spread 63 mm/min
2.5 in/min
(US-FMVSS); ISO 3795
Ineos ABS Lustran® M210TF ABS Pellets
Lustran® ABS M210TF is used in general applications for toy and food contact. It meets European standard EN 71, part 3 and ASTM F 963. It has standard impact strength, high gloss, and is easy flo..