Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flame Spread | 44.0 - 53.0 mm/min | 1.73 - 2.09 in/min | Average value: 48.0 mm/min Grade Count:4 |
Overview of materials for Acetal Homopolymer, Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, Glass Fiber Reinforced". Each property range of values reported is minimum and maxim.. |