Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flame Spread | 12.2 mm/min | 0.480 in/min | FMVSS302 |
Polyram PlusTek PA862 Nylon 6.6 for Injection Molding, High Impact Modified High impact modified Nylon 6.6 for injection molding applications.Information provided by Polyram. |