Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flame Spread | 39.0 mm/min @Thickness 1.00 mm |
1.54 in/min @Thickness 0.0394 in |
FMVSS 302 |
SABIC Innovative Plastics GELOY XP4020R ASA+PC (Asia Pacific) ASA+PC may contain up to 20% post-industrial recycle. Excellent flow, weatherability, toughness and high heat for exterior uses. |
|||
Flame Spread | 39.0 mm/min | 1.54 in/min | |
Dow INSPIRE™ D7000 Thermoplastic Polyolefin
(discontinued **) Information provided by DowThe Inspire brand was spun off from Dow Chemical to Styron in 2010, although this grade had previously been removed from Dow's standard product line. |