Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flame Spread | 1.2 mm/min | 0.047 in/min | 5.0 pcf density |
NOVA Chemicals Arcel 730 70% PS/30% PE Interpolymer ARCEL is a high-performance, moldable foam resin consisting of 70% polystyrene (PS) and 30% polyethylene (PE). ARCEL provides toughness, flexibility and durability in a lightweight foam.The strength.. |