Thermal Properties Metric English Comments
Flame Spread 30.0 mm/min

@Thickness 3.17 mm
1.18 in/min

@Thickness 0.125 in
FH3
LG Chemical 65IH HIPS
High impact, Extrusion, Balanced mechanical properties, Good surface appearance with high gloss, Conforming to FDA CFR 177.1640, Excellent processability, Applications include refrigerator food tray..
Flame Spread 30.0 mm/min
1.18 in/min
Average Extent of Burring; ISO 3795
Styron INSPIREâ„¢ DTF8000 ES Compounded Polypropylene
Overview: INSPIREâ„¢ TF 8000 ES is a superior scratch and mar resistant low gloss talc filled interior grad TPO exhibiting excellent low temperature ductility, high modulus and heat performance.M..
Flame Spread 30.0 mm/min
1.18 in/min
FMVSS 302
Styron MAGNUMâ„¢ 375 HH Acrylonitrile Butadiene Styrene (ABS) Resin
Overview: High Heat, Low Gloss, Medium Impact ABS resin for injection moldingApplications: Automotive interior trim applications requiring low volatile organic compounds (VOC)Information provided by..
Flame Spread 30.0 mm/min
1.18 in/min
FMVSS 302
Styron MAGNUMâ„¢ 375 HP Acrylonitrile Butadiene Styrene (ABS) Resin
Overview: High Heat, Low Gloss, Medium Impact ABS resin for injection molded automotive interior trim applications.Applications: Chrysler-MSDB-191Ford-WSB-M4D690-AGM-GMP.ABS.009Information provided ..