Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flame Spread | 26.0 - 35.0 mm/min | 1.02 - 1.38 in/min | Average value: 27.9 mm/min Grade Count:8 |
Overview of materials for Polystyrene, Molded, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene". Each property range of values reported is minimum and maximum values of appropriate MatWeb.. |
|||
Flame Spread | 26.0 mm/min @Thickness 3.17 mm |
1.02 in/min @Thickness 0.125 in |
FH3 |
LG Chemical 25SPE GPPS Heat resistance, Chemical resistance, Superior transparency and processability, good appearance, non-toxicity (Conforming to FDA CFR 177.1640), Excellent electrical properties, Superior extrusion pr.. |
|||
Flame Spread | 26.0 mm/min @Thickness 3.17 mm |
1.02 in/min @Thickness 0.125 in |
FH3 |
LG Chemical 25SPI GPPS High strength, Superior transparency and processability, good appearance, non-toxicity (Conforming to FDA CFR 177.1640), Excellent electrical properties, Heat resistance and chemical resistance, Sup.. |
|||
Flame Spread | 26.0 mm/min @Thickness 3.17 mm |
1.02 in/min @Thickness 0.125 in |
FH3 |
LG Chemical 25SPR GPPS Superior transparency and processability, good appearance, non-toxicity (Conforming to FDA CFR 177.1640), Excellent electrical properties, Heat resistance and chemical resistance, Superior extrusion.. |