Flame Spread 24.0 mm/min
0.945 in/min
FMVSS 302
Styron MAGNUMâ„¢ 3325 SLG Acrylonitrile Butadiene Styrene (ABS) Resin
Overview: Super Low Gloss, Medium Heat, Medium Impact ABS resin for injection molded automotive interior trim applications Magnum 3325 SLG can achieve 60° Gardner gloss levels below 2.0 with low ..
Flame Spread 24.0 - 100 mm/min
0.945 - 3.94 in/min
Average value: 74.7 mm/min Grade Count:3
Overview of materials for Polybutylene Terephthalate (PBT), Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Bead Filled". Each property range of values reported is minimum ..