Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flame Spread | 22.1 mm/min | 0.870 in/min | FMVSS302 |
Polyram RamOfin PPH343T4BK10 Polypropylene, 20% Mineral Filled 20% Mineral filled, heat resistant polypropylene for injection molding applications.Information provided by Polyram. |
|||
Flame Spread | 22.1 mm/min | 0.870 in/min | FMVSS302 |
Polyram RamOfin PPC343T4 Polypropylene, 20% Mineral Filled 20% Mineral filled, UV stabilized, heat stabilized polypropylene for injection molding applications.Information provided by Polyram. |
|||
Flame Spread | 22.1 mm/min | 0.870 in/min | FMVSS302 |
Polyram RamOfin PPH343T4BK11 Polypropylene, 20% Mineral Filled 20% Mineral filled, UV stabilized, heat resistant polypropylene for injection molding applications.Information provided by Polyram. |