Thermal Properties Metric English Comments
Flame Spread 15.0 mm/min

@Thickness 2.00 mm
0.591 in/min

@Thickness 0.0787 in
FMVSS 302
SABIC Innovative Plastics LNP Thermocomp R1000HI620 PA 66 (Europe-Africa-Middle East)
Impact modified Polyamide 66 injection moulding resin.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Flame Spread 15.0 mm/min

@Thickness 2.00 mm
0.591 in/min

@Thickness 0.0787 in
FMVSS Buring Speed
Eurostar Staramide AST44 PA66, Impact Modified, Injection Molded
AST44 is a Low Temperature Impact Modified Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier.
Flame Spread 15.0 mm/min

@Thickness 2.00 mm
0.591 in/min

@Thickness 0.0787 in
FMVSS Burning Speed
Eurostar Staramide R1000HI620 PA66, Impact Modified, Injection Molded
Staramide R1000HI620 is an Impact Modified Polyamide 66 Injection Molding Resin (also known as R1000HI010)Information provided by Eurostar.