Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flame Spread | 13.4 mm/min | 0.528 in/min | FM VSS-302 |
Multibase Multi-Flex® 1047 Black TPO Thermoplastic Polyolefin Elastomer Forms: PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |