Thermal Properties | Metric | English | Comments |
---|---|---|---|
Decomposition Temperature | 465 °C | 869 °F | Degradation Temperature |
Epoxy Technology EPO-TEK® H55 Epoxy Material Description: A two component, thixotropic and high temperature epoxy designed to be used for hybrids and PCB applications.Information Provided by Epoxy Technology |