Thermal Properties Metric English Comments
Decomposition Temperature 623 °C
1150 °F
10% Weight Loss Temp
UBE UPIMOL® SA101 Heat-Resistant Polyimide Shape
Description: UPIMOL® SA101 is an excellent heat-resistant polyimide shape, based on Biphenyl tetracarboxilic dianhydride(BPDA) originally developed by UBE. UPIMOL® SA101 has improved high durabili..
Decomposition Temperature 623 °C
1150 °F
Daelim H&L Plavis MS Aromatic Polyimide, 15% MoS2 Filled, Machined Parts
Available in vacuum or non-lubrication condition, very high abrasion resistance and low friction coefficient propertyInformation provided by Daelim H&L