Thermal Properties | Metric | English | Comments |
---|---|---|---|
Decomposition Temperature | 324 °C | 615 °F | |
Hybrid Plastics POSS® MA0730 MethacrylFluoro(13)Cyclopentyl-POSS® POSS® Nanostructured Chemical Technology has two unique features: (1) the chemical composition is a hybrid, intermediate (RSiO1.5) between that of silica (SiO2) and silicones (R2SiO). (2) POSS®.. |