Polymer Property : Decomposition Temperature = 502 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Decomposition Temperature 261 °C
502 °F
Degradation Temperature
Epoxy Technology EPO-TEK® 302 Fast Setting, Optical Epoxy
Product Description: EPO-TEK® 302 is a two component, fast-gelling, room temperature curing epoxy, designed for electronic, optical, medical, and general applications. Advantages & Application No..