Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Decomposition Temperature = 487 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Decomposition Temperature 341 - 487 °C
646 - 909 °F
Average value: 405 °C Grade Count:17
Overview of materials for Epoxy, High Temperature
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Encapsulating, Mineral Filled". Each property range of values reported is minimum and maximum val..