Thermal Properties | Metric | English | Comments |
---|---|---|---|
Decomposition Temperature | 444 °C | 831 °F | Degradation Temperature |
Epoxy Technology EPO-TEK® E2036 Epoxy Product Description: A two component, slightly flexible, silver-filled, electrically conductive adhesive for semiconductor and electronic assemblies. It is a low Tg epoxy, intended for many kinds o.. |