Thermal Properties | Metric | English | Comments |
---|---|---|---|
Decomposition Temperature | 443 °C | 829 °F | Degradation Temperature |
Epoxy Technology EPO-TEK® OD2002 High Temperature Epoxy Material Description: High Tg version of EPO-TEK®353ND with low modulus and good toughness. Replacement for EPO-TEK® 364. Complies with USP Class VI biocompatibility standards.Information Provid.. |
|||
Decomposition Temperature | 443 °C | 829 °F | Degradation Temperature |
Epoxy Technology EPO-TEK® OG159-2 UV Cure Optical Epoxy Material Description: A single component, high viscosity, UV curable epoxy adhesive designed for sealing glass plates together in the LCD/OLED/display industry. It contains 1mil glass beads for bon.. |