Thermal Properties | Metric | English | Comments |
---|---|---|---|
Decomposition Temperature | 409 °C | 768 °F | Degradation Temperature |
Epoxy Technology EPO-TEK® 353ND-T Black High Temperature Thixotropic Epoxy Product Description: EPO-TEK® 353ND-T Black is a two component, high temperature, thixotropic epoxy for fiber optic, PCB and various medical applications. Advantages & Application Notes: This produ.. |
|||
Decomposition Temperature | 409 °C | 768 °F | Degradation Temperature |
Epoxy Technology EPO-TEK® 353ND-T High Temperature Thixotropic Epoxy Product Description: EPO TEK® 353ND-T is a two component, highly thixotropic epoxy with non-flowing properties and high temperature resistance. Advantages & Application Notes: Suitable for fiber op.. |
|||
Decomposition Temperature | 409 °C | 768 °F | Degradation Temperature |
Epoxy Technology EPO-TEK® 353ND-T1 High Temperature Thixotropic Epoxy Material Description: A two component, thixotropic and high temperature epoxy designed for fiber optic, electronics and medical applications. It is a more viscous alternative to EPO-TEK® 353ND-T.I.. |
|||
Decomposition Temperature | 409 °C | 768 °F | Degradation Temperature |
Epoxy Technology EPO-TEK® 353ND-T4 Thixotropic Epoxy Product Description: EPO-TEK® 353ND-T4 is a two component, highly thixotropic epoxy with non-flowing properties and high temperature resistance. This is a higher viscosity version of EPO-TEK® 353.. |
|||
Decomposition Temperature | 409 °C | 768 °F | Degradation Temperature |
Epoxy Technology EPO-TEK® 353ND-T5 High Temperature Thixotropic Epoxy Product Description: EPO-TEK® 353ND-T5 is an intermediate viscosity version of EPO-TEK® 353ND and EPO-TEK® 353ND-T. It was designed for high temperature applications in fiber optics, electronics .. |
|||
Decomposition Temperature | 409 °C | 768 °F | Degradation Temperature |
Epoxy Technology EPO-TEK® OG116-31 UV Cure Optical Epoxy Product Description: EPO-TEK® OG116-31 is a single component, UV curable epoxy adhesive and encapsulant, designed for PCB and circuit assembly applications found in semiconductor, computer, medical.. |