Thermal Properties | Metric | English | Comments |
---|---|---|---|
Decomposition Temperature | 406 °C | 763 °F | Degradation Temperature |
Epoxy Technology EPO-TEK® OE138 Two Component Epoxy Material Description: A two component epoxy with intermediate viscosity range between EPO-TEK® 353ND and EPO-TEK® 353ND-T. It is designed for semiconductor glob top applications, as well as use in.. |