Thermal Properties | Metric | English | Comments |
---|---|---|---|
Decomposition Temperature | 3650 °C | 6600 °F | |
Mid-Mountain Materials HYTEX® 5000 High Carbon Industrial Textile (PAN) Description: HYTEX is the trademark for the textile products manufactured by Mid-Mountain Materials, Inc. Hytex high performance textile products are manufactured from various yarns of varying chemi.. |
|||
Decomposition Temperature | 3650 °C | 6600 °F | |
Mid-Mountain Materials HYTEX® 5100 High Carbon Industrial Textile (PAN) Description: HYTEX is the trademark for the textile products manufactured by Mid-Mountain Materials, Inc. Hytex high performance textile products are manufactured from various yarns of varying chemi.. |