Thermal Properties Metric English Comments
Decomposition Temperature 334 °C
633 °F
5% weight loss; TGA; IPC-TM-650.2.4.24.6
Park Electrochemical Nelco® N5000 BT Epoxy Laminate and Prepreg
The Nelco N5000 BT epoxy laminate and prepreg system provides superior electrical properties. The N5000 resin system wasoriginally developed for application specific use in high densitymilitary and ..