Decomposition Temperature 313 °C
595 °F
Degradation Temperature
Epoxy Technology EPO-TEK® B9021 Epoxy Paste
Material Description: A single component, B-stageable epoxy paste for semiconductor, microelectronics, and optical assemblies. It can be used in hybrid assemblies for lid-sealing and substrate atta..