Thermal Properties Metric English Comments
Decomposition Temperature >= 150 °C
>= 302 °F
Solvay Chemicals IXOL® M 125
The polyol IXOL® M125 is a halogenated aliphatic polyether diol. Due to its low functionality, IXOL® M125 is particularly suited for one component polyurethane (PUR) foams or for polyisocyanur..