Thermal Properties | Metric | English | Comments |
---|---|---|---|
Decomposition Temperature | >= 140 °C | >= 284 °F | |
BASF Neopolen® 1702 100 mm Expanded Polyethylene Uses: Foam plates for the production of packaging, sporting goods and technical components.Information provided by BASF |
|||
Decomposition Temperature | >= 140 °C | >= 284 °F | |
BASF Neopolen® 1710 100 mm Expanded Polyethylene Uses: Foam plates for the production of packaging, sporting goods and technical components.Information provided by BASF |
|||
Decomposition Temperature | >= 140 °C | >= 284 °F | |
BASF Neopolen® 1710 120 mm Expanded Polyethylene Uses: Foam plates for the production of packaging, sporting goods and technical components.Information provided by BASF |
|||
Decomposition Temperature | >= 140 °C | >= 284 °F | |
BASF Neopolen® 1710 50 mm Expanded Polyethylene Uses: Foam plates for the production of packaging, sporting goods and technical components.Information provided by BASF |
|||
Decomposition Temperature | >= 140 °C | >= 284 °F | |
BASF Neopolen® 1710 60 mm Expanded Polyethylene Uses: Foam plates for the production of packaging, sporting goods and technical components.Information provided by BASF |
|||
Decomposition Temperature | >= 140 °C | >= 284 °F | |
BASF Neopolen® 1712 100 mm Expanded Polyethylene Uses: Foam plates for the production of packaging, sporting goods and technical components.Information provided by BASF |
|||
Decomposition Temperature | >= 140 °C | >= 284 °F | |
BASF Neopolen® 1710 40 mm Expanded Polyethylene Uses: Foam plates for the production of packaging, sporting goods and technical components.Information provided by BASF |