Decomposition Temperature 230 °C
446 °F
Dow ISONATE™ 125M Pure MDI
ISONATE™ 125M is a crystalline, pure MDI mixture is characterized by high purity, low acidity and reproducible reactivity. This di-functional product is a key ingredient in preparing prepolymers f..
Decomposition Temperature 230 °C
446 °F
Dow ISONATE™ 125MDR Pure MDI
ISONATE™ 125MDR is a crystalline, pure MDI mixture is characterized by high purity, low acidity and reproducible reactivity. This difunctional product is a key ingredient in preparing prepolymers ..
Decomposition Temperature 230 °C
446 °F
Dow ISONATE™ 143L Modified MDI
ISONATE™ 143L modified MDI is a polycarbodiimide-modified diphenylmethane diisocyanate.Information provided by Dow
Decomposition Temperature 230 °C
446 °F
Dow ISONATE™ 143L Modified MDI
ISONATE™ 143 is a polycarbodiimide-modified diphenylmethane diisocyanate. Liquid at room temperature, this product has a low viscosity and good storage stability down to 75°F. The polycarbodiimi..
Decomposition Temperature 230 °C
446 °F
Dow ISONATE™ 181 MDI Prepolymer
ISONATE™ 181 MDI prepolymer is a modified MDI compound produced by reacting high-purity diphenylmethane diisocyanate with sufficient glycol to allow easy handling down to 80°F. This medium-viscos..
Decomposition Temperature 230 °C
446 °F
Dow ISONATE™ 240 MDI Prepolymer
ISONATE™ 240 MDI prepolymer is a modified MDI compound produced by reacting high-purity diphenylmethane diisocyanate with a high molecular weight polyester polyol, resulting in a material with good..
Decomposition Temperature 230 °C
446 °F
Dow ISONATE™ 50 O,P` Pure MDI
ISONATE™ 50 O,P` is a high ortho-para MDI designed for use in polyurethane adhesives, sealants, sports flooring, coatings, electrical encapsulants and flexible molded foams. ISONATE™ 50 O,P` offe..
Decomposition Temperature 230 °C
446 °F
Dow PAPI™ 901 Polymeric MDI
PAPI™ 901 polymeric MDI is a polymethylene polyphenylisocyanate that contains MDI. This product has a high functionality and a high viscosity resulting in highly rigid foams. This product is desi..
Decomposition Temperature 230 °C
446 °F
Dow PAPI™ 94 Polymeric MDI
PAPI™ 901 polymeric MDI is a polymethylene polyphenylisocyanate that contains MDI. This products low viscosity, low functionality, increased diphenylmethane diisocyanate content and increased perc..
Decomposition Temperature 230 °C
446 °F
Dow PAPI™ 95 Polymeric MDI
PAPI™ 95 polymeric MDI is a polymethylene polyphenylisocyanate that contains MDI. This product`s functionality (value of 2.4) and viscosity have been optimized by maintaining a high diphenylmethan..
Decomposition Temperature 230 °C
446 °F
Dow ISONATE™ 181 MDI Prepolymer
ISONATE™ 181 MDI prepolymer is a modified MDI compound produced by reacting high-purity diphenylmethane diisocyanate with sufficient glycol to allow easy handling down to 80°F. This medium-viscos..
Decomposition Temperature 230 °C
446 °F
Dow PAPI™ 20 Polymeric MDI
PAPI™ 20 polymeric MDI is a polymethylene polyphenylisocyanate that contains MDI. This product`s functionality value of 3.2 and high viscosity result in highly rigid foams. This product is design..
Decomposition Temperature 230 °C
446 °F
Dow PAPI™ 580 N Polymeric MDI
PAPI™ 580 N polymeric MDI is a polymethylene polyphenylisocyanate that contains MDI. This product has high functionality (value of 3.0) and relatively high viscosity. Recommended for use in polyi..
Decomposition Temperature 230 °C
446 °F
Dow PAPI™ 27 Polymeric MDI
PAPI™ 27 polymeric MDI is a polymethylene polyphenylisocyanate that contains MDI. This product has a narrow molecular weight distribution and a high reactivity. Applicable to many foam processes,..