Thermal Properties Metric English Comments
Decomposition Temperature 70.0 °C
158 °F
ASTM D648
Wanshijie PETG Sheet
PETG is also named GPET. It is made of a kind of non-crystalline PET resin sourced from cyclohexanediol modification. PETG differs greatly from PET and PCT. PETG is a kind of non-crystalline copolym..