Thermal Properties | Metric | English | Comments |
---|---|---|---|
Decomposition Temperature | 555 °C | 1030 °F | 5 percent; IPC TM-650 2.4.24.6 |
Arlon AD300C Commercial Microwave and RF Laminate Material Excellent Thermal Coefficient of Dielectric Constant (TCEr = -25 ppm/°C)Excellent PIM performanceHigh Thermal Conductivity ideal for Higher Power DesignsReduced Coefficient of Thermal Expansion in .. |
|||
Decomposition Temperature | 554 °C | 1030 °F | 5 percent; IPC TM-650 2.4.24.6 |
Arlon CLTE-XT High Precision Ceramic PTFE Microwave material for improved thermal management, Excellent dimensional stability with high degree of phase stability vs. temperature.CLTE-XT is a micro-dispersed ceramic PTFE composite utilizing .. |