Thermal Properties | Metric | English | Comments |
---|---|---|---|
Decomposition Temperature | 540 °C | 1000 °F | ASTM E1131 |
Zeus PEEK Tubing PEEK (polyetheretherketone) is a high-performance engineered polymer with excellent endurance to heat and one of the highest strength-to-weight ratios of any thermoplastic. This material can be used.. |