Polymer Property : Flash Point = 79.9 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Flash Point 26.6 °C
79.9 °F
closed cup
Dow Corning Z-6121 SILANE
Dow Corning® Z-6121 Silane is a multi-purpose silane adhesion promoter recommended for use with epoxy coatings, silicone resin-based coatings and alkyd finishes.Information provided by Dow Corning