Thermal Properties Metric English Comments
Flash Point 23.9 °C
75.0 °F
Aremco Pyro-Paint™ 634-YO High Temperature Refractory Coating, YO >95%
This ultra high temperature yttrium oxide coating provides exceptional protection of graphite, ceramic and metal components exposed to reactive molten metals such as titanium, uranium and their allo..