Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flash Point | 360 °C | 680 °F | ASTM D1929 |
Dalau Dalcon 025 75% Virgin PTFE, 25% Glass Fiber, Blue Applications & Industries: General: 25% Glass fibre is the most widely used filler. It improves the creep resistance, compressive strength, rigidity, and wear of PTFE, both at low & high temperature.. |
|||