Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flash Point | 63.9 °C | 147 °F | Method A; ASTM D93 |
ExxonMobil Exxsol™ D60 Dearomatized Fluid Availability: Africa & Middle East, Asia Pacific, Europe, Central America, North America and South AmericaAppearance: Clear/Transparent LiquidInformation provided by ExxonMobil |
|||
Flash Point | 63.9 °C | 147 °F | ASTM D93 |
ExxonMobil Isopar™ L (AP) Isoparaffin Fluid Product Description: A clear isoparaffin fluid, typically containing less than 1 ppm benzene and less than 1 ppm sulfur. Appearance: Clear/Transparent LiquidAvailability: Asia PacificInformation pro.. |
|||
Flash Point | 63.9 °C | 147 °F | Method A; ASTM D93 |
ExxonMobil Solvesso™ 150 ND Aromatic Fluid Appearance: Clear/Transparent LiquidAvailability: Africa & Middle East, Europe, Asia Pacific, Central America, North America and South AmericaInformation provided by ExxonMobil |
|||
Flash Point | 63.9 °C | 147 °F | ASTM D56 |
ExxonMobil Varsol™ 140 Naphtha Non-dearomatized Fluid Appearance: Clear/Transparent LiquidAvailability: North AmericaInformation provided by ExxonMobil |