Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flash Point | 56.1 °C | 133 °F | ASTM D56 |
ExxonMobil Isopar™ K (AM) Isoparaffin Fluid Product Description: A clear isoparaffin fluid, typically containing less than 1 ppm benzene and less than 1 ppm sulfur. Appearance: Clear/Transparent LiquidAvailability: North AmericaInformation pr.. |