Polymer Property : Flash Point = 538 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Flash Point 281 °C
538 °F
ASTM D92
ExxonMobil Teresstic 220
TERESSTIC is the brand name for a line of long-service-life lubricating oils that have ranked for over five decades among the finest products of their kind. Continually improved over the years, TERE..
Flash Point 281 °C
538 °F
ASTM D92
ExxonMobil Teresstic 320
TERESSTIC is the brand name for a line of long-service-life lubricating oils that have ranked for over five decades among the finest products of their kind. Continually improved over the years, TERE..
Flash Point 281 °C
538 °F
COC; ASTM D92
ExxonMobil SpectraSyn™ 40 Polyalphaolefin (PAO) Fluid
Product Description: SpectraSyn™ High Viscosity Polyalphaolefin (PAO) basestocks feature low temperature properties (pour point and viscosity), low volatility, and improved thermal stability. Spect..
Flash Point 281 °C
538 °F
ASTM D92
ExxonMobil Teresstic 220
TERESSTIC is the brand name for a line of long-service-life lubricating oils that have ranked for over five decades among the finest products of their kind. Continually improved over the years, TERE..
Flash Point 281 °C
538 °F
ASTM D92
ExxonMobil Teresstic 320
TERESSTIC is the brand name for a line of long-service-life lubricating oils that have ranked for over five decades among the finest products of their kind. Continually improved over the years, TERE..