Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flash Point | 253 °C | 487 °F | ASTM D92 |
ExxonMobil 80 Exxon Aviation Oil EE Series Aviation Oil EE is the brand name of a premium quality line of ashless-dispersant piston engine oils. Formulated with select, highly refined base oils together with ashless-dispersant and anti-oxida.. |
|||
Flash Point | 253 °C | 487 °F | ASTM D92 |
ExxonMobil Mobil 1 10W-40 Motorcycle Oil MX4T 4-Cycle Mobil 1 Motorcycle Oils are formulated with 100 percent synthetic fluids. The unique, synthetic structure of the Mobil 1 Motorcycle formulations enable them to offer advantages well beyond conventio.. |
|||
Flash Point | 253 °C | 487 °F | ASTM D92 |
ChevronTexaco ParaMount™ 3005 Paraffinic Process Oil FeaturesChevron’s ParaMount Paraffinic Process Oils are highly saturated paraffinic process oils with very good color and low aromatic content.Chevron’s modern all-hydroprocessing technology assur.. |
|||
Flash Point | 253 °C | 487 °F | ASTM D92 |
ExxonMobil 80 Exxon Aviation Oil EE Series Aviation Oil EE is the brand name of a premium quality line of ashless-dispersant piston engine oils. Formulated with select, highly refined base oils together with ashless-dispersant and anti-oxida.. |
|||
Flash Point | 253 °C | 487 °F | ASTM D92 |
ExxonMobil Mobil 1 10W-40 Motorcycle Oil MX4T 4-Cycle Mobil 1 Motorcycle Oils are formulated with 100 percent synthetic fluids. The unique, synthetic structure of the Mobil 1 Motorcycle formulations enable them to offer advantages well beyond conventio.. |