Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flash Point | 208 °C | 406 °F | ASTM D92 |
ChevronTexaco Elite-Cut® AM Metal Working Fluid FeaturesChevron -Cut Metalworking Fluids are a complete line of chlorinated cutting oils. The line consists of individual products with antiweld and lubricity properties to cover practically all met.. |
|||
Flash Point | 208 °C | 406 °F | ASTM D92 |
ChevronTexaco ParaMount™ 1005 Paraffinic Process Oil FeaturesChevron’s ParaMount Paraffinic Process Oils are highly saturated paraffinic process oils with very good color and low aromatic content.Chevron’s modern all-hydroprocessing technology assur.. |
|||
Flash Point | 208 °C | 406 °F | |
ChevronTexaco Quenchtex® B Texaco Quenchtex oils deliver value through:Controlled cooling of metals — Combines the high initial quenching speed of water with slow final quenching speed of oil.Safety — High flash point and f.. |
|||
Flash Point | 208 °C | 406 °F | |
ELM® SoyFluid™ Hydraulic All Season Premium Biodegradable - Biobased Hydraulic Oil Description: ELM Biotechbased SoyFluid Hydraulic All Season Oil is a biodegradable hydraulic oil formulated with the best optimized USA grown natural seed oils that surpass the lubricity of most con.. |