Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flash Point | 4.44 °C | 40.0 °F | |
Lord Adhesives 459T Toluene Adhesion Promoter for Lord Acrylic, Epoxy, Urethane and Cyanoacrylate Adhesives To meet the unique bonding demands that accompany the use of difficult-to-bond materials, the Lord Corporation offers a full line of adhesion enhancers/surface modifiers. Lord® Adhesion Enhancers.. |