Polymer Property : Flash Point = 3700 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Flash Point >= 2038 °C
>= 3700 °F
Pyrotek Pyrocast FSC-2000 Stabilized fused silica cement
Pyrocast FSC-2000 eliminates the need for cement pre-mixing or rolling while providing the same outstanding characteristics of all dense fused silica products.ApplicationsAdhesive Coating Patching c..