Thermal Properties Metric English Comments
Flash Point 178 °C
352 °F
ASTM D92
ExxonMobil 80W-140 Mobilube HD
Mobilube HD 80W-140 is a heavy-duty gear lubricant formulated from high performance base oils and an advanced additive system. This lubricant is engineered for commercial axles and final drives wher..
Flash Point 178 °C
352 °F
ASTM D92
ExxonMobil 80W-140 Mobilube HD
Mobilube HD 80W-140 is a heavy-duty gear lubricant formulated from high performance base oils and an advanced additive system. This lubricant is engineered for commercial axles and final drives wher..
Flash Point 178 °C
352 °F
ASTM D92
ChevronTexaco ISO 32 Machine Oil R&O LVI
FeaturesChevron Machine Oil R&O LVI is a superior quality naphthenic lubricating oilIt is formulated with highly refined base stock with rust inhibiting, antioxidant, and foam suppressant additives...