Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flash Point | 33.3 °C | 92.0 °F | |
Lord Adhesives 7707 n-Butyl Acetate Surface Conditioner Lord Adhesion Enhancers/Surface ModifiersTo meet the unique bonding demands that accompany the use of difficult-to-bond materials, the Lord Corporation offers a full line of adhesion enhancers/surfa.. |
|||
Flash Point | 33.3 °C | 91.9 °F | Setaflash, Closed Cup; ASTM D3278-82 |
Lord Adhesives Aeroglaze® Z3480 High Solids Aromatic Polyurethane Coating Aeroglaze® Z3480 coating is designed for use on properly prepared and primed metal surfaces, in regions requiring a VOC below 335.8 g/l (2.8 lbs/gallon).All information provided by Lord. |