Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flash Point | 316 °C | 601 °F | ASTM D92 |
ChevronTexaco ISO 680 Cylinder Oil W FeaturesChevron Cylinder Oils W are designed to meet the needs of emulsifying cylinder oils.Chevron Cylinder Oils W provide excellent metal wettability. The combination of oil emulsibility and metal.. |
|||
Flash Point | 316 °C | 601 °F | ASTM D92 |
ChevronTexaco ParaMount™ ELV Paraffinic Process Oil FeaturesChevron ParaMount ELV Paraffinic Process Oil offers all the advantages of a bright stock including low weight loss and excellent solubility.ELV is exceptional because of its very light color.. |
|||
Flash Point | 316 °C | 601 °F | |
ChevronTexaco Vanguard® 680 Texaco Vanguard oils deliver value through:Excellent metal wettability and high film strength for any moisture condition.Versatility — Three viscosity grades available to cover the range of steam p.. |
|||
Flash Point | 316 °C | 600 °F | |
ConocoPhillips Inca® 1000 Oil, AGMA No. 8A Comp. Description: Conoco Inca Oil is a high-quality compounded lubricant recommended for use in heavily loaded industrial and automotive worm gears and bearings operating at moderate to high temperatures.. |
|||
Flash Point | >= 316 °C | >= 600 °F | ASTM D 92 |
ConocoPhillips 680 Bearing Oil Description: Conoco Bearing Oil is formulated for the circulating systems that lubricate roll-neck bearings in steel and nonferrous rolling mills. It is suited for systems in which water and corrosi.. |