Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flash Point | 157 °C | 315 °F | |
Lubriplate Low Pour Petroleum-Based Heavy-Duty Hydraulic Oil ISO 22 petroleum-based oil for low temperature applications. Low Temp Hydraulic Oils are available in Jugs, Pails, 1/4 Drums & Drums.Information provided by Lubriplate |
|||
Flash Point | 157 °C | 315 °F | |
ConocoPhillips Transformer Oil Description: Conoco Transformer Oil, an insulating oil of very high dielectric strength, is suited for oil-filled transformers in both large substations and small pole-mounted transformers. It is al.. |
|||
Flash Point | 157 °C | 315 °F | COC; ASTM D92 |
ExxonMobil SpectraSyn™ 2 Polyalphaolefin (PAO) Fluid Product Description: SpectraSyn™ Low Viscosity Polyalphaolefin (PAO) basestocks feature low temperature properties, low volatility, and improved thermal stability. SpectraSyn™ Low Viscosity (PAO) .. |
|||
Flash Point | 157 °C | 315 °F | |
BASF N,N’-Dimethylurea Formula: C3H8N2OCAS: 96-31-1Description Dimethylurea is a colorless to white powder, with an amine-like odor.Synonyms: 1,3-DimethylureaApplications: Intermediate used in the production of Pharmaceut.. |