Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flash Point | 308 °C | 586 °F | |
ELM® SoyFluid™ Hydraulic Industrial (ISO 68) Premium Biodegradable – Biobased Hydraulic Oil Description: ELM Biotechbased SoyFluid™ Hydraulic Industrial (ISO 46 & 68) are biodegradable hydraulic oils formulated with the best optimized USA grown natural seed oils that surpass the lubricity.. |
|||
Flash Point | 308 °C | 586 °F | ASTM D92 |
ChevronTexaco ISO 460 Cylinder Oil W FeaturesChevron Cylinder Oils W are designed to meet the needs of emulsifying cylinder oils.Chevron Cylinder Oils W provide excellent metal wettability. The combination of oil emulsibility and metal.. |
|||
Flash Point | 308 °C | 586 °F | ASTM D92 |
ChevronTexaco Regal® 390 Texaco Regal oil delivers value through:Long lubricant life provided by good natural thermal and oxidation stability.Good demulsibility, which assures good lubricant, film strength and reduced wear .. |
|||
Flash Point | 308 °C | 586 °F | |
ChevronTexaco Vanguard® 460 Texaco Vanguard oils deliver value through:Excellent metal wettability and high film strength for any moisture condition.Versatility — Three viscosity grades available to cover the range of steam p.. |