Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flash Point | 294 °C | 561 °F | ASTM D92 |
ExxonMobil Mobil EAL 224H Mobil EAL 224H is a premium performance environmentally aware hydraulic fluid designed to provide outstanding performance in hydraulic and circulation systems operating at moderate conditions. It pr.. |
|||
Flash Point | 294 °C | 561 °F | ASTM D92 |
ChevronTexaco ISO 220 AIO FeaturesChevron AIO (Chevron Authentic Industrial Oils) provide rust protection, oxidation inhibition, and foam suppression.Chevron AIO are good quality lubricants for any application not requiring .. |
|||
Flash Point | 294 °C | 561 °F | ASTM D92 |
ChevronTexaco Regal® 220 R&O Texaco Regal R&O oils deliver value through:Prolonged oil service life — Excellent oxidation stability provided by the multi-component inhibitor system resists oil breakdown during exposure to high.. |
|||
Flash Point | 294 °C | 561 °F | ASTM D92 |
ExxonMobil Mobil EAL 224H Mobil EAL 224H is a premium performance environmentally aware hydraulic fluid designed to provide outstanding performance in hydraulic and circulation systems operating at moderate conditions. It pr.. |
|||
Flash Point | 294 °C | 561 °F | ASTM D92 |
ChevronTexaco Regal® 220 Texaco Regal oil delivers value through:Long lubricant life provided by good natural thermal and oxidation stability.Good demulsibility, which assures good lubricant, film strength and reduced wear .. |