Polymer Property : Flash Point = 286 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Flash Point 141 °C
286 °F
ChevronTexaco Meropa® 3200
Texaco Meropa oils deliver value through:Gear set efficiencies — High thermal stability EP system maintains clean gear and bearing surfaces, minimizing deposits which interfere with effective lubri..
Flash Point 141 °C
286 °F
Closed Cup
Solvay RHODISOLV® INFINITY Solvent
Description: Rhodiasolv INFINITY is a blend of dibasic ester solvent and proprietary surfactantsChemical Name: Microemulsion concentrate based on dimethyl-2-methyl glutarateSolubility in water: 100%..