Polymer Property : Flash Point = 286 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Flash Point 286 °C
547 °F
Teknor Apex TruVis Esters™ TTDTM Tri-Tridecyl Trimellitate
Flash Point 286 °C
547 °F
ASTM D92
ExxonMobil Mobil Vaculine 546
Mobil Vacuoline 500 Series are extra high performance heavy duty circulating oils specifically designed to meet the critical requirements of the Morgan Construction Companys high speed No-Twist® Ro..
Flash Point 286 °C
547 °F
ASTM D92
ExxonMobil Mobil Vaculine 548
Mobil Vacuoline 500 Series are extra high performance heavy duty circulating oils specifically designed to meet the critical requirements of the Morgan Construction Companys high speed No-Twist® Ro..
Flash Point 286 °C
547 °F
ASTM D92
ExxonMobil Mobil Vaculine 137
The Mobil Vacuoline 100 range is a series of extra high quality circulating system oils primarily intended for the lubrication of plain bearings in systems designed for full fluid lubrication, parti..
Flash Point 286 °C
547 °F
ASTM D92
ExxonMobil AA Mobil DTE Oil Double Letter Series
The Mobil DTE Oil Double Letter Series of lubricants are high performance heavy duty circulating oils primarily intended for continuous reuse in circulation lubrication systems for gears and bearing..
Flash Point 286 °C
547 °F
ASTM D92
ExxonMobil Mobil Vaculine 137
The Mobil Vacuoline 100 range is a series of extra high quality circulating system oils primarily intended for the lubrication of plain bearings in systems designed for full fluid lubrication, parti..
Flash Point 286 °C
547 °F
ASTM D92
ExxonMobil Mobil Vaculine 546
Mobil Vacuoline 500 Series are extra high performance heavy duty circulating oils specifically designed to meet the critical requirements of the Morgan Construction Companys high speed No-Twist® Ro..
Flash Point 286 °C
547 °F
ASTM D92
ExxonMobil Mobil Vaculine 548
Mobil Vacuoline 500 Series are extra high performance heavy duty circulating oils specifically designed to meet the critical requirements of the Morgan Construction Companys high speed No-Twist® Ro..
Flash Point 286 °C
547 °F
ASTM D92
ChevronTexaco Rykon® ISO 46 Premium Oil
FeaturesChevron Rykon Premium Oils are designed to give maximum protection to hydraulic pumps.They are formulated with ISOSYN® base stocks incorporating antiwear additives, oxidation and corrosion ..
Flash Point 286 °C
547 °F
ASTM D92
ExxonMobil AA Mobil DTE Oil Double Letter Series
The Mobil DTE Oil Double Letter Series of lubricants are high performance heavy duty circulating oils primarily intended for continuous reuse in circulation lubrication systems for gears and bearing..