Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flash Point | 283 °C | 541 °F | COC; ASTM D92 |
ExxonMobil SpectraSyn™ 100 Polyalphaolefin (PAO) Fluid Product Description: SpectraSyn™ High Viscosity Polyalphaolefin (PAO) basestocks feature low temperature properties (pour point and viscosity), low volatility, and improved thermal stability. Spect.. |